改質(zhì)瀝青對(duì)電煅無(wú)煙煤和瀝青焦浸潤(rùn)性的研究
發(fā)布時(shí)間:2018-10-08 14:41
【摘要】:以改質(zhì)瀝青為粘結(jié)劑、電煅無(wú)煙煤和瀝青焦為骨料,研究骨料粒度、加熱溫度、保溫時(shí)間及振動(dòng)次數(shù)對(duì)改質(zhì)瀝青浸潤(rùn)性的影響,并對(duì)不同粒度分布的電煅無(wú)煙煤和瀝青焦的比表面積進(jìn)行測(cè)定。結(jié)果表明,隨著骨料粒度的減小,骨料顆粒的比表面積逐漸增大;改質(zhì)瀝青對(duì)電煅無(wú)煙煤和瀝青焦的浸潤(rùn)性均隨骨料粒度的減小和振動(dòng)次數(shù)的增加而大幅度降低,隨加熱溫度和保溫時(shí)間的增加而逐漸增大。通過(guò)適當(dāng)調(diào)整骨料粒度分布、加熱溫度、保溫時(shí)間、振動(dòng)次數(shù)等工藝參數(shù),能夠改善改質(zhì)瀝青對(duì)電煅無(wú)煙煤和瀝青焦的浸潤(rùn)效果。
[Abstract]:Using modified asphalt as binder and electric calcined anthracite and bituminous coke as aggregate, the effects of aggregate size, heating temperature, holding time and vibration times on the wettability of modified bitumen were studied. The specific surface area of electric calcined anthracite and bituminous coke with different particle size distribution was measured. The results show that the specific surface area of aggregate particle increases with the decrease of aggregate particle size, and the wettability of modified asphalt to electrically calcined anthracite and bituminous coke decreases greatly with the decrease of aggregate particle size and the increase of vibration times. With the increase of heating temperature and holding time, it increases gradually. The wetting effect of modified bitumen on electric calcined anthracite and bituminous coke can be improved by adjusting the particle size distribution of aggregate, heating temperature, holding time, vibration times and other technological parameters.
【作者單位】: 貴州師范大學(xué)材料與建筑工程學(xué)院;貴州省鋁電解炭素材料工程技術(shù)研究中心;貴州省教育廳無(wú)機(jī)非金屬功能材料重點(diǎn)實(shí)驗(yàn)室;
【基金】:貴州省科學(xué)技術(shù)基金(黔科合J字[2013]2221號(hào)) 貴州省教育廳專(zhuān)業(yè)綜合改革試點(diǎn)項(xiàng)目(黔教高發(fā)[2013]446) 貴陽(yáng)市白云區(qū)科技計(jì)劃項(xiàng)目(白科合同[2013]40號(hào))
【分類(lèi)號(hào)】:TF821;TQ127.11
本文編號(hào):2257147
[Abstract]:Using modified asphalt as binder and electric calcined anthracite and bituminous coke as aggregate, the effects of aggregate size, heating temperature, holding time and vibration times on the wettability of modified bitumen were studied. The specific surface area of electric calcined anthracite and bituminous coke with different particle size distribution was measured. The results show that the specific surface area of aggregate particle increases with the decrease of aggregate particle size, and the wettability of modified asphalt to electrically calcined anthracite and bituminous coke decreases greatly with the decrease of aggregate particle size and the increase of vibration times. With the increase of heating temperature and holding time, it increases gradually. The wetting effect of modified bitumen on electric calcined anthracite and bituminous coke can be improved by adjusting the particle size distribution of aggregate, heating temperature, holding time, vibration times and other technological parameters.
【作者單位】: 貴州師范大學(xué)材料與建筑工程學(xué)院;貴州省鋁電解炭素材料工程技術(shù)研究中心;貴州省教育廳無(wú)機(jī)非金屬功能材料重點(diǎn)實(shí)驗(yàn)室;
【基金】:貴州省科學(xué)技術(shù)基金(黔科合J字[2013]2221號(hào)) 貴州省教育廳專(zhuān)業(yè)綜合改革試點(diǎn)項(xiàng)目(黔教高發(fā)[2013]446) 貴陽(yáng)市白云區(qū)科技計(jì)劃項(xiàng)目(白科合同[2013]40號(hào))
【分類(lèi)號(hào)】:TF821;TQ127.11
【相似文獻(xiàn)】
相關(guān)期刊論文 前6條
1 馮勇祥;改質(zhì)瀝青在東碳公司的應(yīng)用[J];炭素;2003年03期
2 雷滋森;生產(chǎn)改質(zhì)瀝青提高炭素制品質(zhì)量[J];炭素;2000年03期
3 李鐵虎,,楊崢,喬生儒,鄭修麟;用改質(zhì)瀝青制備碳-石墨材料的研究[J];機(jī)械工程材料;1994年01期
4 ;文摘[J];炭素技術(shù);2003年01期
5 傅亮;劉存貴;李現(xiàn)芳;;改質(zhì)瀝青輸送泵的改進(jìn)[J];設(shè)備管理與維修;2011年10期
6 劉麟,趙秀芳,劉欣;YB/T5194-1993改質(zhì)瀝青行業(yè)標(biāo)準(zhǔn)制(修)訂[J];冶金標(biāo)準(zhǔn)化與質(zhì)量;2005年04期