超輕頁巖陶粒混凝土性能分析
本文選題:頁巖陶粒 + 超輕; 參考:《混凝土》2017年05期
【摘要】:以混凝土滿足和易性、強度的同時表觀密度最小為目標,在保證混凝土強度達到墻板抗拉開裂最大強度的前提下,配制出一系列表觀密度不大于900 kg/m~3超輕混凝土,并且探索特殊外加劑對混凝土的影響。通過15種配合比試驗,得出最佳配合比。充分利用粉煤灰、煤矸石等工業(yè)廢料,真正實現(xiàn)變廢為寶。
[Abstract]:Aiming at the satisfaction and easiness of concrete and the minimum apparent density at the same time of strength, a series of ultra-light concrete with apparent density less than 900 kg/m~3 were prepared under the premise of ensuring that the strength of concrete reached the maximum tensile cracking strength of the wall slab.The influence of special admixture on concrete is also explored.The optimum mixture ratio was obtained by 15 kinds of mixture ratio tests.Make full use of fly ash, coal gangue and other industrial wastes, and truly realize the transformation of waste into treasure.
【作者單位】: 太原理工大學(xué)建筑與土木工程學(xué)院;
【基金】:國家自然青年科學(xué)基金項目(51208332)
【分類號】:TU528.2
【相似文獻】
相關(guān)期刊論文 前6條
1 梁欣欣;劉道永;;頁巖陶粒混凝土受壓性能分析[J];科技風(fēng);2010年22期
2 王璇;王磊;;頁巖陶;炷恋呐浜媳仍O(shè)計及性能的試驗研究[J];四川建材;2012年05期
3 余火勝;劉松柏;;高性能頁巖陶;炷恋目杀眯匝芯縖J];江西建材;2013年02期
4 黃昱霖;嚴云;李三霞;;低成本大流動度輕質(zhì)高強頁巖陶;炷裂芯縖J];新型建筑材料;2011年01期
5 盧紅;;碎石型頁巖陶;炷恋牧W(xué)性能和工作性能研究[J];福建建筑;2014年02期
6 ;[J];;年期
相關(guān)會議論文 前2條
1 宋術(shù)杰;鄭秀華;謝寧;;礦物摻合料對頁巖陶;炷量箟簭姸鹊挠绊慬A];輕骨料工業(yè)發(fā)展及工程應(yīng)用——第十一屆全國輕骨料及輕骨料混凝土學(xué)術(shù)討論會暨第五屆海峽兩岸輕骨料混凝土產(chǎn)制與應(yīng)用技術(shù)研討會論文集[C];2012年
2 鄭秀華;袁杰;葛勇;張寶生;;預(yù)濕程度對頁巖陶;炷翉姸群涂箖鲂缘挠绊慬A];輕骨料工業(yè)發(fā)展及工程應(yīng)用——第十一屆全國輕骨料及輕骨料混凝土學(xué)術(shù)討論會暨第五屆海峽兩岸輕骨料混凝土產(chǎn)制與應(yīng)用技術(shù)研討會論文集[C];2012年
相關(guān)碩士學(xué)位論文 前2條
1 張鵬;高強混凝土和頁巖陶;炷恋娜S受壓破壞準則[D];河南理工大學(xué);2014年
2 劉陽杰;碎石型頁巖陶;炷恋闹苽渑c性能研究[D];南昌大學(xué);2012年